Rejuvenating "Torque-Seal"
Thread Starter

Joined: Apr 2000
Posts: 438
Likes: 3
From: South of YSSY
Rejuvenating "Torque-Seal"
Have a few tubes of orange "Torque-Seal" which have gone a bit stiff and "plasticene-like" in the tubes. Anyone know how to re-liquify them or do we just chuck 'em?
Joined: Apr 2010
Posts: 65
Likes: 0
From: London, England
Anyone know how to re-liquify them or do we just chuck 'em?
Joined: Apr 2010
Posts: 65
Likes: 0
From: London, England
Actually, thinking about it, if it doesn't tell you what the solvent is on the label, you might be able to get an idea from the smell.
I'm not sure this is a good idea for anything critical though. If it flakes or something, you may end up having to replace it all. I am right in thinking it's only purpose is to show whether a fitting has been tampered with? If it is supposed to actually hold the fastener (like Loctite etc), I certainly wouldn't try to 'revive' it if I was going to use it on anything more important than a toilet door hinge...
I'm not sure this is a good idea for anything critical though. If it flakes or something, you may end up having to replace it all. I am right in thinking it's only purpose is to show whether a fitting has been tampered with? If it is supposed to actually hold the fastener (like Loctite etc), I certainly wouldn't try to 'revive' it if I was going to use it on anything more important than a toilet door hinge...
Thread Starter

Joined: Apr 2000
Posts: 438
Likes: 3
From: South of YSSY
"Torque-Seal" is just a visual indicator that a fastener or component has remained undisturbed since it was applied. A thin bead is usually laid across the surfaces (such as a nut on the end of a bolt, of the bottom of an oil-filter against the fitting etc) and this facilitates a quick visual inspection.
Haven't tried the acetone yet but that is a pretty decent organic solvent. The toluene did soften it up to the point it would extrude from the nozzle.
Haven't tried the acetone yet but that is a pretty decent organic solvent. The toluene did soften it up to the point it would extrude from the nozzle.

Joined: Jan 2008
Aviation Qualifications: SLF
Posts: 58
Likes: 1
From: Frome - where we do as Fromans do
google remains your friend
You might find some very useful information here...
http://www.dtic.mil/cgi-bin/GetTRDoc...c=GetTRDoc.pdf
jg
http://www.dtic.mil/cgi-bin/GetTRDoc...c=GetTRDoc.pdf
jg