White layer is a hard but brittle iron nitride intermetallic compound that forms as a surface layer during nitriding. Being brittle, if the layer is thick enough, it can crack and thus form the start of a fatigue crack. Hence nitridng specs allow a maximum thickness - and at University I sucked at metallurgy, so thats all I know.